The platinic solution is added drop wise to the MOF slurry and stirred for 1 day at room temperature. The resulting material is recovered by filtration and washed twice with methanol and dried in air at 333 K.
The platinic solution is added dropwise to the MOF slurry and stirred for 1 day at room temperature.The resulting material is recovered by filtration and washed twicewith methanol and dried in air at 333 K.