The as-processed
NG Ti has an average grain size of 80 nm which was elaborated in
our previous report [10]. Using a muffle furnace with a temperature
accuracy of 71 1C in the hot zone, the NG Ti was annealed at
500 1C for 5, 10, 20, 30, 40, 50 and 60 min