From the statistical analysis of the discontinuous assay, it can be said that Cellulose is significantly different from Agrobiofilm®1, for P < 0.05 level of significance. On our equipment with continuous aeration and CO2 analysis, the biodegradation rate is increased when comparing to the batch system and for 72 days of assay, the increase was 55.8%.