The results
showed that the maximum adsorption capacity was obtained
when the ceramic adsorbent was sintered at 600 C for 1.5 h. Finally,
the granular ceramic product was cooled to 105 C and sieved to
a diameter of 2–3 mm and then kept in an airtight plastic tube under
room temperature for further use.