About testing EN-7210.
- Send report hull cell testing Nimuden-DX compare with EN-7210.
- Nimuden-DX can plating in hull cell 1 MTO (80 min.) and after that is have plate out.
- EN-7210 can plating in hull cell 5 MTO (450 min.).
- Present Nimuden-DX is have lead but EN-7210 product is lead free (improved RoHS )
- Price of EN-7210 is less than Nimuden-DX (last meeting we send running cost to K.Pinai).
- Show hull cell plate of Nimuden-DX and EN-7210 for compare brightness.
- On testing we will record and make report for summarize to A.L.M.T. .
- A.L.M.T. need hardness around 600 HV., Show TDS of EN-7210 to K.Pinai this product hardness around 900-1,000 HV by heat treatment.
- Time of testing, We will testing until renew it can compare long life of solution.
- On testing new make up Nimuden-DX and EN-7210, Start plating together and part plating is same for easy to compare.
Result :
About testing EN-7210.
- Now the customer building lab room and line not complete , If building finish we will start testing.
- K.Pinai will inform more detail about our product to Japanese manager
- I will check preparedness with K.Pinai again on next week.