BSG were sterilized at 120 °C for 15min prior treatment. They were then used in their original form and after delignification. Delignification was performed according to Bardi and Koutinas (1994).
BSG were sterilized at 120 °C for 15min prior treatment.They were then used in their original form and after delignification.Delignification was performed according toBardi and Koutinas (1994).