The resulting polymer was condensed in water, grinded, and
washed with water. Then it was immersed in 10 wt% NaOH aqueous
solution for 20 h while stirring to eliminate remaining polyphosphoric
acid and then washed until neutral pH was attained. Finally
it was dried at 90 ◦C.