Surface temperature as a function of time: (A) 15 min of electrospun PCL/
PCM fibres deposition stored at 4 C; (B) 15 min of electrospun PCL/PCM fibres
deposition and 15 min of electrospun PCL fibres stored at 4 C; (C) and (D) 45 min of
electrospun PCL/PCM fibres deposition stored at 25 and 4 C, respectively; (E) and
(F) 45 min of electrospun PCL/PCM fibres deposition and 15 min of electrospun PCL
fibres stored at 25 and 4 C, respectively.