The structural alignment of PB/CdS/CNT ensures the simplest pathway
for the mass diffusion and electron shuttle, and a high surface area accessible to the chemical and electrochemical reactions,
so as to minimize the concentration- and electrochemicalpolarization and thus ensure the fast overall kinetics of the electrode reaction.