commercial pure Al (99.7%, all compositions quoted in this work are in wt.% unless otherwise stated), commercial pure crystalline Si (99.9%) and commercial pure Mg (99.8%) were used as starting materials to prepare Ale10%Mg2Si alloy in a 25 kW medium fre-quency induction furnace. The alloy was remelted at 750