As
the filler agglomeration is less for compatibilized blends, the filler
particles can be properly wetted by macromolecules and hence
adhesion between the filler and matrix improves. Thus, the energy
required to propagate a crack increases, resulting in higher tear strength [40]. The values show a decreasing tendency as the MA
concentration further goes up.