To this solution was added 70 ml of chloroacetic acid. The
mixture was stirred at 90 oC for 1 hour. After cooling to room
temperature, the polymer was precipitated by cold ethanol,
dissolved in a solution of sodium carbonate in acetone and
reprecipitated [2] several times into ethanol (Scheme -2).