preparation of catalyst by dry impregnation after support briun at temperature 550 2 hr to get rid of the impurities mixed in a solute of sodium carbonate 45% dry at temperature 120 16 hr bryer temperature 550 5 hr the catalyst received to keep it in Disiccator before test reaction