The grain size distribution of the FA and the CCR compared with that of the silty clay is shown in Fig. 2. The curves were obtained from laser particle size analysis. The D50 of the FA is0.0035 mm, which is close to that of the clay, and the D50 of the CCR is 0.01 mm (2.5 times larger than that of the clay).