Addition of the WS fibers alone or in combination with PLA-g-MA, did not significantly change the glass transition (Tg) and melting temperature (Tm) of the PLA, which were around 60 and 170 8C, respectively
Additionof the WS fibers alone or in combination with PLA-g-MA,did not significantly change the glass transition (Tg) andmelting temperature (Tm) of the PLA, which were around60 and 170 8C, respectively