Methods. Spin-coated films were prepared with a Mikasa MS-A100
spin coater. A drop of polymer solutions (100 g dm−3) containing
either HPIP (1) or 6-cyano HPIP (2; 0.5 w/w% with respect to
polymer) were spin-coated at 1000 rpm onto quartz plates and then