The spherical structure was retained with nearly the same pore size and smooth pore margins, even when the calcination temperature was increased to 6508C (Figure 2 b)
The spherical structure was retained with nearly the same pore sizeand smooth pore margins, even when the calcination temperaturewas increased to 6508C (Figure 2 b)