Tests on the wet polymer sample using the compression
mode, at different heating rates (in the graphics, at
°C.min1
). a) experimental results using plates with 15 mm
diameter; b) heating rate dependence on the measured onset
temperature of the water melting (the inset graphics shows the
dependence on the measured onset temperature obtained with
plates of different diameters, at 4 °C.min1