Forging. Heat to I I50 “C (2 100 “F). Do not forge below 8 I5 “C ( 1500 ‘F) Recommended Heat Treating Practice Normalizing. Heat to 855 “C (1570 “F). Cool in air
Forging. Heat to I I50 “C (2 100 “F). Do not forge below 8 I5 “C ( 1500 ‘F)Recommended Heat Treating PracticeNormalizing. Heat to 855 “C (1570 “F). Cool in air