when a viltage is applied to the battery with such polarity that the positive terminal of the source goes to the plate having the nickel hydroxide ( positive ) , and the negative goes to the plate with rhe cadmium hydroxide ( negative ) , oxygen is driven from the negative plate , leaving metallic cadmium.