Peel off color and Red rust meeting. Last time, they got feedback from Kubota (Vietnam) that found NG part (Peel off color) on wheels. It is wheel production on May’2016, customer need to know root cause to protect this problem to next time and do not let happen again.
In meeting, they inform new problem about red rust after pre-treatment before baking. I explain factor and suggest to them already. Right now, I will bring all data to join meeting with team.