however, this range would be led to a
reduction of EPS volume and varies the proper test circumstance
leading a miss-leading value of water absorption. So a lower temperature
range is utilized to subside this phenomenon. After drying
of samples they submerged in the water for 72 h to measure the increased
weight. Another reason for this observation could be