For composites with modified bentonite, it can be seen in Table 1 that interlayer spacing is bigger for lower clay content (i.e., d = 4.30 nm for PBAT with 3% mod. bentonite and d = 3.52 nm for PBAT with 5% mod. bentonite). It can be concluded that better dispersion can be achieved for lower filler contents.