EDX analysis confirmed that the desired structure could
be obtained. Although sub-micron powder and 20–40 lm powder
of iron oxide were used to study the effect of the iron oxide nominal cluster size on reactivity, a clear conclusion could not be made
since some agglomeration of the sub-micron powder took place
during the preparation resulting in little difference between actual
cluster sizes.