Anodization to form tube layers is usually carried out by applying a potential step (or ramp) at a constant voltage
between 1–30 V in aqueous electrolyte or 5–150 V in nonaqueous electrolytes containing approximately 0.05m–0.5m
(0.1–1 wt%) fluoride ions (and usually some background ion species).