From this study, SCBA calcined at 600°C has good pozzolanic properties, suggesting suitability
for use in cement. The replacement of 10% cement with SCBA effectively increases the
compressive strength. The increase in the use of SCBA could reduce environmental problems
and minimize the requirement of landfill area to dispose of the SCBA.