cellulose was dispersed after the solvent was pre-cooled to −10 ◦ C, followed by vigorously stirring for 3 min. The solution temperature was then maintained between −2 to 0 ◦ C using a saltice bath and the mixture was vigorously stirred for 7 min to obtain transparent cellulose dope (referred to as method II).