For a typical procedure, 10 g F127 copolymer was mixed with 85 g ethanol. The resulting solution was heated up to 40 C to form a clear solution under stirring.
For a typical procedure, 10 g F127 copolymer was mixed with85 g ethanol. The resulting solution was heated up to 40 C toform a clear solution under stirring.