Over a 28-day incubation period of the two strains on PE films, viable biofilms formed, and the PE films’ hydrophobicity decreased. Obvious damage, including pits and cavities (0.3−0.4 μm in depth), was observed on the surfaces of the PE films using scanning electron microscopy (SEM) and atomic force microscopy (AFM)