Unlike spin coating the area can be easily scaled up and the material usage is almost 100%. Furthermore, not only single layer but also multilayer can be deposited without a buffer
liquid.
The single layer PLED performance is as good as that of the spin coated one. The bilayer PLED is even better than the one by liquid buffer method.