The papers were cut into 22 mm 40 mm pieces for contact
angle and ATR-IR measurements, 65 mm 65 mm for PPS
roughness and sto¨ ckigt sizing degree, 25 mm 180 mm for wet
tensile strength test and dried in an oven at 103 8C for 2 h to keep
papers free of water.