According to related researches, cells can become degraded or defective due to high temperature during the thermal treatment and the inorganic acids used during the nitric acid dissolution process. It is also reported that the cell-protecting thermal treat- ment of Si modules with wafers of thickness less than 200 μm is very tricky.