The average iron oxide crystallite
size for the unpromoted supported catalysts was determined
by line broadening analysis of XRD (X-ray diffraction) patterns obtained
with a Bruker AXS D8 ADVANCE diffractometer equipped
with a CoKa1 source (k = 0.1789 nm) using an angle range from
20 to 90 in 2h.