The materials used in this study were: Portland-composite cement with blast furnace slag CP II E 32 (defined by NBR 11578/1997 [15] as containing: 56% < clinker + calcium sulfate < 94%; 6% < blast furnace slag < 34%; 0% < filler < 10%), quartz sand, basalt stone, sugarcane bagasse ash sand (SBAS) and construction waste (CW)