In case of TPA parameters of the RF/TS blend gels (Fig. 1), it was
found that hardness tended to increase with increasing RF ratio
until reaching the maximum value (71 N) at RF:TS blending ratio
of 50:50, whose TPA profile was resemble to that of pure TS but
with the higher compressibility (Fig. 2).