Samples for TEM analysis were mechanically polished to 30 μm thick, punched to a disk of 3 mm diameter by a copper disk cutter and then jet polished to thin foil specimens in perchloric acid
(10%) and acetic acid (90%) mixture under 20 V at 15 °C. The electrical conductivity was measured using Microhmmeter (DO5000 series).