The reagents were chosen to prepare activated carbon with different pore sizes and surface structures. Activation with K2CO3 required a high temperature (800◦ C) for the heating process, however, the temperature was lower (450◦ C) for activation in the presence of H3PO4.The activated carbon samples were used as electrode materials in supercapacitors.