Yesterday
1.Plean
- Feiti : Today, they are normal production and appearance on parts was OK! but need to increase plating time from 56 mins to 58 mins to thickness complete (checked Zinc = 7 g/L, NaOH 120 g/L.)
2.Bu
- Prem Sub : Nickel tank No.2 have a problem about surface not smooth with occur grain on parts. Solve this problem by using carbon filter and dummy on morning and start production again on afternoon, they can plating is normally.
- Khlonglung Chromium : Order epuwat-Y17 to adjust in nickel all 3 tank to solving on part.
- Thai Switch Gear : Customer maybe order epclen-51 to try and next time they would like to sampling of Tin Bight to analyes in our lab (currently use Auto Tech)