Therefore,
if some Sb volatilizes during the processing the material
will show negative Seebeck coefficient. Further, the more
Sb volatilizes, the bigger the absolute value of the Seebeck
coefficient will be. As the temperature increases the intrinsic
conduction is generated and major carriers become holes;
therefore the conduction type of the CoSb3 sample changes
from n-type to p-type.