The XRD analysis of the fired film was carried out in the range of 2 = 20–80◦. The XRD (Fig. 2) analysis shows the spinel structure with phases as NiMn2O4 (average intensity = 43%), CoMn2O4 (average intensity = 13%), and NiCo2O4 (average intensity = 4%). The