The pressed mats were kept under
compression for 24 h by bolting the two steel plates together using
four 15 mm thick bolts. After 24 h, the boards were declamped,
stacked vertically and conditioned for 28 days at 20
±
1 ◦C and
65
±
5% RH to allow the cement to cure and gain strength.