From modulated DSC results, it was found that the degree of crystallinity of the PET
samples employed in this work varied from 40.7% down to 2.1%. After
plasma treatment, the surfaces of the 4 different PET foils became
more hydrophilic as indicated by a decrease in water contact angle.