Owing to the contribution of SDS to the increase in
the number of negative charges on the surface particles
as already mentioned, the presence of SDS in the peroxide-
prevulcanised latex also resulted in a higher CTC
value (4.70±0.04·10–5) compared to that of the latex
without SDS (4.10±0.03·10–5) and of the uncured
latex.