The thermal stress tests were performed for a duration from 3
to 9 h. The electrical stress test was performed with a continuous
biased DC current with density of 6.5 104 mA/lm2 for a duration
from 3 to 9 h. Finally, the contact resistances were measured
after the thermal and electrical treatments to evaluate the stability
of the contacts.