Tensile testing analysis of the PLA-g-MA (8:2)
revealed that the strength was reduced from 69 (that of the
neat PLA) to 49MPa of the compatibilizer, suggesting that
the presence of the free radical initiator and MA in PLA
causes drastic reduction in the tensile properties