Following ASTM C 349, the specimen 28-day compressive strength was measured using portions of the prisms broken in the above-mentioned flexural test.
The specimen contact surface area was 40 40 mm2. Six specimens, as a group, were tested for obtaining average compressive strength along with the standard deviation.