over average magnetic flux density, Bave, of the single bulk is higher than that of stacked bulks in each scanning height. On the other hand, the trapped flux area over Bave of the stacked bulks is almost 4 % larger than that of single one. There is a trade-off between the strength and the area of the trapped magnetic field.