The temperature of the substrate should be minimum 10°C and at least 3°C above the dew point of the air,
temperature and relative humidity measured in the vicinity of the substrate. Good ventilation is required in confined
areas to ensure proper drying. The coating should not be exposed to oil, chemicals or mechanical stress until cured.