2) The silica was pre-compounded with PP at 200°C for 5 min. Then the obtained material (PP/silica) was blended with the second polymer during a second extrusion step.
2) The silica was pre-compounded with PP at 200°C for 5 min. Then the obtained material (PP/silica) wasblended with the second polymer during a second extrusion step.