Comparing the results of laboratory research on the application of collector Flotigam DAT with results obtained
with the application of Aero 3030C in the flotation concentration of feldspar and mica on sample ‘‘Bujanovac’’, it can be concluded:
• For flotation of mica from raw material ‘‘Bujanovac’’, collector Armoflot 64 or Aero 3030C may be
used. The quality and recovery of mica in both cases are satisfactory.
• For flotation of feldspar better recoveries were obtained with the application of the collector Aero
3030C (19.58%) than with collector Flotigam DAT (6.18%). Furthermore, the quality of feldspar and quartz sand was satisfactory regardless of which reagent was used.